- Problem 1000 Y 0 6 Chypoeutectoid Plain Carbon Steel Is Slowly Cooled From 950 C To A Temperature Just Slightly Below 1 (44.69 KiB) Viewed 24 times
Problem 1000 Y 0.6% Chypoeutectoid plain- carbon steel is slowly cooled from 950°C to a temperature just slightly below
-
- Site Admin
- Posts: 899603
- Joined: Mon Aug 02, 2021 8:13 am
Problem 1000 Y 0.6% Chypoeutectoid plain- carbon steel is slowly cooled from 950°C to a temperature just slightly below
Problem 1000 Y 0.6% Chypoeutectoid plain- carbon steel is slowly cooled from 950°C to a temperature just slightly below 723°C. 900 800 ya b Y+ FC 0.02 723°C Temperature (°C) 700 600 (a) Calculate the weight percent proeutectoid ferrite in the steel. rec (b) Calculate the weight percent eutectoid ferrite and eutectoid cementite in the steel. 500 + Fec Pearlite 400 0.8 6.67 0 100% Fe 0.6 Weight percent carbon