- Q5 We Want To Use Thermal Evaporation To Deposit A Platinum Layer On Top Of The Structures Shown Below If The Formed T 1 (23.33 KiB) Viewed 40 times
Q5. We want to use thermal evaporation to deposit a platinum layer on top of the structures shown below. If the formed t
-
- Site Admin
- Posts: 899603
- Joined: Mon Aug 02, 2021 8:13 am
Q5. We want to use thermal evaporation to deposit a platinum layer on top of the structures shown below. If the formed t
Q5. We want to use thermal evaporation to deposit a platinum layer on top of the structures shown below. If the formed thickness on the flat surface is 200nm, calculate the film thickness on the labeled surfaces (i.e. A, B, and C) for the cases shown below. Ⓒ flat surface 120 flat surface flat surface 135 flat surface (a) No Source (b) Source