= = A. AISI 1050 Hot Rolled steel shaft (Syield = 37.5 kpsi; Sultimate = 68 kpsi) as in Figure 4 is used in engine components in airplanes. Shafts are made with lathes. The steel shaft is subjected to a load of P = 6000 lb. Pure alternating voltage occurs on the shaft when rotating. The shaft operates at a temperature of 250 F. Determine the safety factor against fatigue failure in the part where there is a fillet 1/16R. Will the part suffer from fatigue failure? a B. Mention and describe the types of loads that can cause fatigue failure in engine components