An FCC iron-carbon alloy initially containing 0.20 wt\% C is carburized at an elevated temperature and in an atmosphere
Posted: Fri Jul 15, 2022 4:45 pm
this is the only data
An FCC iron-carbon alloy initially containing 0.20 wt\% C is carburized at an elevated temperature and in an atmosphere wherein the surface carbon concentration is maintained at 1.0wt% C. If after 49.5 h the concentration of carbon is 0.45 wt\% C at a position 4.0 mm below the surface, determine the temperature in degree Celsius (∘C) at which the treatment was carried out.
An FCC iron-carbon alloy initially containing 0.20 wt\% C is carburized at an elevated temperature and in an atmosphere wherein the surface carbon concentration is maintained at 1.0wt% C. If after 49.5 h the concentration of carbon is 0.45 wt\% C at a position 4.0 mm below the surface, determine the temperature in degree Celsius (∘C) at which the treatment was carried out.