The charge to a Portland cement rotary kiln contains 33.50 % CO, 42.50 % CaO, 13.00 % SiO,, 8.00 % Fe₂O3,3.0 % MgO. The
Posted: Fri Jul 08, 2022 6:09 am
The charge to a Portland cement rotary kiln contains 33.50 % CO, 42.50 % CaO, 13.00 % SiO,, 8.00 % Fe₂O3,3.0 % MgO. The coke used is hydrogen free and dry and contains 8 % ash. The clinkers contains 63. 42 % CaO3,28 % MgO, 11.42 % Fe₂O3, Al₂O3 and 21.88 % SiO₂ and the flue gas contains 31.3 % CO₂, 1.8 % O₂ and the balance nitrogen. Calculate per 100 kg of clinker a. Kg Charge b. Kg coke c. Kmol air d. Kmol flue gas