2. The parabolic rate coefficient at 1200 °C wet oxidation is 0.920 µm²/hr. If it took 120 minutes to grow the initial o
Posted: Tue May 24, 2022 11:23 am
2. The parabolic rate coefficient at 1200 °C wet oxidation is 0.920 µm²/hr. If it took 120 minutes to grow the initial oxide, for how long (in hours) should the wafer be subjected to another oxidation process to grow an 25000 Aº thick oxide? (4 points)