1. You are given an equilibrium-solidified Al-Cu alloy indicated in Figure 1. Please advise a heat treatment procedure t
-
answerhappygod
- Site Admin
- Posts: 899604
- Joined: Mon Aug 02, 2021 8:13 am
1. You are given an equilibrium-solidified Al-Cu alloy indicated in Figure 1. Please advise a heat treatment procedure t
1. You are given an equilibrium-solidified Al-Cu alloy indicated in Figure 1. Please advise a heat treatment procedure that can be used to achieve a maximum strength without losing a significant amount of ductility. Please draw your temperature history in the temperature-time coordinate beside the phase diagram and describe the microstructure change in each heat treatment step. (40 pts) 800 L CALO) 600 La 548 C Temperature (°C) 400 LL Temperature (°C) a+0 0 0 10 Fig. 1 SO 60 20 30 40 Copper (wt%) Time